1 of 44

Wrought Metals��

2 of 44

Aims and objectives

  • Know the difference between cast and wrought base metal alloy

​

  • Manufacturing of wrought metals
  • Know dental applications of wrought base metal alloy
  • Identify their properties and the role of various alloying elements

3 of 44

General Requirements

​

  1. Should not produce harmful toxic or allergic effects
  2. Resistance to corrosion and physical changes when in the oral fluids.
  3. The physical and mechanical properties, such as thermal conductivity, melting temperature, coefficient of thermal expansion, and strength, should all be satisfactory
  4. Easy to process and handle.
  5. Relatively inexpensive, and readily available.

4 of 44

​

A cast alloy is when the molten alloy is poured into a mold to give it its shape.

A wrought alloy is one that is worked by being forged or hammered.

​

​

�

Photomicrograph of cold-worked gold, showing deformed grains and slip lines (the parallel lines within grains) at surface offsets where dislocations have exited their slip planes (×100). (Courtesy of S. D. Tylman.)

5 of 44

Cast alloys

Wrought alloys

​

Cast cobalt-chromium alloys

  • Removable dental prosthesis framework
  • Ceramic-metal restorations

Cast nickel-chromium alloys

  • Ceramic-metal restorations

Cast titanium and titanium alloys

  • Crowns
  • Fixed partial prosthesis
  • Removable dental prosthesis framework
  • Implants

​

Wrought titanium and titanium alloys

  • Implants
  • Crowns
  • Fixed partial prosthesis

Wrought stainless steel alloys

  • Endodontic instruments
  • Orthodontic wires and brackets
  • Preformed crowns

Wrought cobalt-chromium-nickel alloys

  • orthodontic wires
  • endodontic files

Wrought nickel-titanium alloys

  • orthodontic wires
  • endodontic files

Wrought beta Ti alloys( Ti/Mo)

  • orthodontic wires

​

​

6 of 44

Wrought Alloys

  • Alloys that are worked/shaped and adapted into prefabricated forms for use in dental restorations are described as wrought alloys

​

  • The work done to the alloy is usually at a temperature far below the melting point and is therefore referred to as cold work.

​

  • The physical properties required of the wrought alloy will depend on the technique used and the composition of the alloy in the existing prosthesis.

​

​

​

​

​

​

​

7 of 44

​

Examples of some processes:

​

  • Round wires are obtained by drawing a cast alloy through series of dies
  • Rolling to form sheets
  • Forging is a process by compression against two dies. E.g. SS crowns

​

8 of 44

The microstructure of wrought alloys is fibrous. Due to the cold work

applied during the operations that shape the alloy into its final form.

9 of 44

1-Cold working: The process of plastically deforming metal at room temperature

  • This method of manufacture results in a tremendous amount of stress (work hardening).

​

  • This stress is relieved by heat treatment.

Grains are elongated in the direction of stretching

10 of 44

Advantages of wrought alloys over cast alloys:

​

​

​

​

​

A wrought alloy is stronger as it has been cold-worked, pounded into shape. It may have been heated and then cooled slowly to anneal it to make it stronger. Between working it and annealing it the molecules are brought closer together giving it more strength.

Disadvantages:

Reduced ductility Increased corrosion

​

11 of 44

2-Annealing:

​

Occurs when heat is applied to metal that has been work-hardened. Raising the temperature allows diffusion to take place at a faster rate. This changes the structure to a lower energy configuration.

​

Three processes are recognised:

1. Recovery

2. Recrystallization

3. Grain Growth

12 of 44

13 of 44

14 of 44

15 of 44

16 of 44

Wrought alloys types

Wrought alloys can be either:

  • Gold wrought alloys
  • Base-metal wrought alloys:
  • Stainless Steel (SS)
  • Co-Cr-Nickle
  • Nickle-Titanium
  • Beta-Titanium

​

17 of 44

Wrought Stainless Steel Alloys

  • Steel is an iron-carbon alloy.
  • Stainless steel are alloys of iron and carbon that contain chromium, nickel, manganese, and other metals to improve properties and give the stainless quality to the steel.
  • Usually, stainless steel alloys are not cast, but instead are used in the wrought form.
  • Applications include: Orthodontic appliances and fabrication of endodontic instruments, such as files and reamers, temporary space maintainers, prefabricated crowns, and the various clinical and laboratory instruments.

18 of 44

Ferritic SS �

​

  • Chromium steels employed in the manufacture of instruments or equipment parts in which some degree of tarnish resistance is desirable.
  • Amounts of chromium, may vary from 15% to 25%.
  • Elements such as carbon, silicon, and molybdenum within narrow limits.
  • Stable at temperature up to 912 ◦ C.
  • cannot be heat treated or hardened.
  • Little dental applications.

​

​

​

​

​

​

​

​

​

19 of 44

Martensitic SS�

​

  • Primarily chromium steels with a lower chromium content (about 12% to 18%).
  • Can be hardened to some degree by heat treatment
  • Have a moderate resistance to tarnish.
  • used in the construction of surgical and cutting instruments, orthodontic appliances, endo instruments and crowns for paediatric patients

​

​

​

​

​

​

​

​

​

​

20 of 44

​

Austenitic SS ( 18/8 SS)

​

  • Chromium 18% and nickel 8%, carbon (0.08% and 0.20%), titanium, manganese, silicon, molybdenum, niobium, and tantalum (in minor amounts) to give important modifications to the properties.
  • (= 72%) iron.
  • Have the highest corrosion resistance.
  • It is the most commonly used alloy for orthodontic stainless steel wires and bands.

21 of 44

22 of 44

23 of 44

Function of Alloying Elements ��Chromium

  • The corrosion resistance of stainless steel is attributed to presence of chromium in the alloy.

​

  • 11% chromium is needed to produce corrosion resistance in pure iron, and the necessary proportion is increased with the addition of carbon to form steel.

24 of 44

  • Chromium resists corrosion well because of the formation of a strongly adherent coating of oxide on the surface, which prevents further reaction with the metal below the surface. The formation of such an oxide layer is called passivation
  • Passivity is influenced by a number of factors: alloy composition, heat treatment, surface condition, stress in the prosthesis, and the environment in which the prosthesis is placed.
  • In dental applications, the stainless characteristics of the alloys can be altered or lost by many ways: excessive heating during assembly or adaptation; using abrasives or reactive cleaning agents, which can alter the surface conditions of the prosthesis; and even by poor oral hygiene practices over prolonged periods.

​

​

​

25 of 44

Function of Alloying Elements and chemical resistance��Chromium

  • If there is more than 28% chromium, chromium carbides instead of oxide form at the grain boundaries, producing a brittle alloy and decrease corrosion resistance in a process known as sensitization.
  • Stabilized stainless steels, contain titanium, niobium, or tantalum, so the carbides that do form are titanium carbides rather than chromium carbides. Those elements prevent the formation of chromium carbides in a process known as stabilisation.

26 of 44

Function of Alloying Elements and chemical resistance��Heat treatment

  • Heat treatment above 650° C results in recrystallization of the microstructure, compositional changes, and formation of chromium-carbides, three factors that can reduce mechanical properties and corrosion resistance.
  • Heat treatment between 400° and 500° C for 5 to 120 seconds, removes the effects of cold working during fabrication, increase ductility, or produce some degree of hardening with some alloys

27 of 44

Function of Alloying Elements and chemical resistance ��Other factors�

  • Molybdenum increases the resistance to pitting corrosion.
  • The chemical resistance of stainless steel alloys is improved if the surface is clean, smooth, and polished. Irregularities promote electrochemical action on the surface of the alloy.
  • Soldering operations on stainless steel with gold and silver solder may contribute to a reduction in stainless qualities because of electrogalvanic action between dissimilar metals or because of localized, improper composition of the stainless steel wire.

​

28 of 44

Uses of SS wrought alloys in dentistry��SS orthodontic wires

  • Cold worked using pliers, resulting in increase yield strength from 275 to 1100 MPa.
  • Heat treatment on 400-500 ◦C is recommended to remove the internal stress of the wire to prevent the premature breakage. It also increases the elastic limit and hardness.
  • The annealing procedure should be carried out only with ‘stabilized’ stainless steel wires which contain small quantities of titanium.
  • Soldering is difficult and requires skill.

​

​

29 of 44

SS prefabricated crowns

  • SS crowns are recommended to restore primary teeth.
  • Have reasonable strength and hardness.

​

30 of 44

SS endodontic instruments

  • Numerous endodontic instruments are classified for hand use or as motor-driven instruments.
  • The most common instruments are the K type of root canal files and reamers. These are manufactured by machining a stainless steel wire into a pyramidal blank, either square or triangular in cross section, and then twisting the blank to form a spiral cutting edge.
  • A file with a rhombohedral cross section has also been introduced.

​

​

31 of 44

  • Mechanical properties are dependent on file geometry, direction of loading and composition. e.g Rhomohedral are less stiff than K-files. Both are weaked in counterclockwise, so twist <¼ turn.

​

32 of 44

Wrought alloys types

  • Base-metal wrought alloys:
  • Stainless Steel (SS)
  • Co-Cr-Nickle
  • Nickle-Titanium
  • Beta-Titanium

​

33 of 44

Wrought Co/Cr/Ni alloy

  • 40% Co, 20% Cr, 15% Ni, and some other elements.
  • Used for Orthodontic wires
  • Formed and shaped then heat-treated for 7 min at 482 ͦC.
  • Wiptam (round Co-Cr wire) wires can be attached to the RPD framework

​

​

34 of 44

Comparison between cast and wrought�cobalt-chromium clasps

​

Cast

Wrought

Yeild strength, MPa.

550

1200

Elongation to fracture, %.

<5

12

​

Young’s modulus, GPa

230

230

Shaped by

Casting

Bending

Fixed to framework by

Integral

Solder

Section shape may be

Tapered

Uniform

35 of 44

Wrought alloys types

  • Base-metal wrought alloys:
  • Stainless Steel (SS)
  • Co-Cr-Nickle
  • Nickle-Titanium
  • Beta-Titanium

​

36 of 44

Wrought Nickel-Titanium Alloy

  • known as Nitinol is used as a wire for orthodontic appliances.
  • Nitinol is characterized by its high resiliency, limited formability, and thermal memory.
  • 55% Ni, 45% Ti.
  • Possesses a temperature transition range (TTR). At temperatures below the TTR, the alloy can be deformed plastically. When the alloy is then heated from below to above the TTR, a temperature-induced crystallographic transformation from a martensitic to an austenitic microstructure occurs and the alloy will return to its original shape. Hence, nickel-titanium is called a shape-memory alloy.
  • Comparable properties to stainless steel and a beta-titanium alloy in tension, bending, and torsion but the lowest elastic modulus and yield strength and the highest spring-back (maximum elastic deflection) of all.

37 of 44

Nickel-Titanium Endodontic instruments

  • Nitinol contains about 56% Ni and 44% Ti by weight. In some instances, <2% of cobalt may be substituted for nickel
  • These alloys can change their structure from austenitic (body-centered cubic) to martensitic (close-packed hexagonal) as a function of stress during root canal preparation.
  • The modulus of Ni-Ti austenite is 120 GPa, and that of martensite is 50 GPa. This effect results in what is termed super-elasticity, and when stress is removed the alloy returns to original shape without permanent deformation and the alloy becomes austenite again.

​

​

38 of 44

  • The super-elasticity of Ni-Ti permits deformations of 8% strain in endodontic files with complete recovery (only less than 1% is allowed in SS alloys).

​

  • Has higher strength, lower elastic modulus and comparable corrosion resistance to SS.

39 of 44

Wrought alloys types

  • Base-metal wrought alloys:
  • Stainless Steel (SS)
  • Co-Cr-Nickle
  • Nickle-Titanium
  • Beta-Titanium

​

40 of 44

Wrought Beta-Titanium Alloy

  • A titanium-molybdenum alloy known as betatitanium is used as a wrought orthodontic wire.
  • Beta-titanium alloy for dental use has the composition 78% titanium, 11.5% molybdenum, 6% zirconium, and 4.5% tin and is supplied as wrought wire.
  • Compared with stainless steel wires, beta-titanium wire has lower force magnitudes, a lower elastic modulus, higher springback (maximum elastic deflection), a lower yield strength, and good ductility, weldability, and corrosion resistance.
  • Its formability and weldability are advantages over Nitinol, and it has a larger working range than do stainless steel wires.

41 of 44

Keywords for your knowledge

  • Annealing—The process of controlled heating and cooling that is designed to produce desired properties in a metal. Typically, the annealing process is intended to soften metals, to increase their ductility, stabilize shape, and increase machinability (see stress relief). In the case of gold foil, the term refers to removal of contaminant from the surface of the foil.
  • Cold welding—The process of joining metals by metallic bonding. The metal-joining process does not occur by heating or fusion but by pressure applied to the interface between the two parts to be joined; no liquid or molten phase is produced witihn the interface joint.
  • Cold working—The process of plastically deforming metal at room temperature.
  • Compaction (condensation)—The process of increasing the density of metal foil, pellets, or powder through compressive pressure.
  • Degassing—The process of removing gases (or other impurities) from the surface of a solid or liquid, usually by heating.
  • Desorption—The process of removing molecules that have attached to the surface of a solid by a physical or chemical action; it is a broader term than degassing.
  • Dislocation—An imperfection in the crystalline arrangement of atoms consisting of either an extra partial plane of atoms (edge dislocation), a spiral distortion of normally parallel atom planes (screw dislocation), or a combination of the two types.
  • Ductility—The ability of a solid to be elongated or thinned plastically without fracturing.
  • Ductile fracture—The rupture of a solid structure resulting in measurable plastic deformation.

​

42 of 44

  • Grain growth—The increase in the mean crystal size of a polycrystalline metal produced by a heat-treatment process.
  • Grain refinement—The process of reducing the crystal (grain) size in a solid metal through the action of specific alloying elements or compounds.
  • Interstitial atom—An imperfection in a crystal lattice consisting of an extra atom located between the adjacent atoms in normal lattice sites.
  • Malleability—The ability (of a metal) to be hammered into thin sheets without fracturing.
  • Point defect—A lattice imperfection of atomic size in three dimensions, such as a vacancy, divacancy, trivacancy, or interstitial atom.
  • Precipitation hardening—The process of strengthening and hardening a metal by precipitating a phase or constituent from a saturated solid solution.
  • Recovery—A stage of heat treatment that results in the partial restoration of properties of a work-hardened metal without a change in the grain structure.
  • Recrystallization—The process of forming new stress-free crystals in a work-hardened metal through a controlled heat-treatment process.
  • Springback—The amount of elastic strain that a metal can recover when loaded to and unloaded from its yield strength; an important property of orthodontic wires.
  • Strain hardening—The increase in strength and hardness and decrease in ductility of a metal that is caused by plastic deformation below its recrystallization temperature; also called work hardening.

​

43 of 44

  • Stress relief—The reduction of residual stress by heat treatment.
  • Superelasticity—The ability of certain nickel-titanium alloys to undergo extensive deformation resulting from a stress-assisted phase transformation, with the reverse transformation occurring on unloading; sometimes called pseudoelasticity.
  • Vacancy—An imperfection in a crystal lattice consisting of an unoccupied atom site.
  • Work hardening—See strain hardening.
  • Working range—The maximum amount of elastic strain that an orthodontic wire can sustain before it plastically deforms.
  • Wrought metal—A metal that has been plastically deformed to alter the shape of the structure and certain mechanical properties, such as strength, hardness, and ductility.
  • �

​

44 of 44

​

​

​

Thank you

r.amoush@ju.edu.jo